Research Article

Alumina Template-Dependant Growth of Cobalt Nanowire Arrays

Figure 3

Top view FESEM images for fragments of Co nw arrays fabricated under the optimized AC deposition conditions in the sulfuric acid alumina template pores after the template etching in 0.5 M for (a) 30, (b) 70 and (c) 100 minutes.
149691.fig.003a
(a)
149691.fig.003b
(b)
149691.fig.003c
(c)