Variation of the amount of Co ( ) inside the alumina pores for the deposition solution made of 0.2 , 0.7 , 0.01 M , and TEA up to pH 5.7, at constant AC voltage of 32 V, 50 Hz and 20 oC, as a function of the deposition time. 15 nm; template thickness ( ) 15 m. In the inset, variation of versus AC frequency (f) for the same deposition solution and value for 15 minutes of deposition.