The typical damage of blade under 30° impact.
(a) 350 m/s “piece out”
(b) 280 m/s “piece out”
(c) 200 m/s “torn”
(d) 160 m/s “torn”
(e) 140 m/s “dented”
(f) 120 m/s “dented”
(g) 100 m/s “nicked”