Emulsion Electrospinning as an Approach to Fabricate PLGA/Chitosan Nanofibers for Biomedical Applications

Figure 3

SEM images of PLGA (16%)/chitosan (4%)/PVA (8%) nanofibrous mats prepared using various voltages of (a) 8 kV, (b) 12 kV, and (c) 16 kV (feed rate = 0.25 mL/h, tip to collector distance = 15 cm).