Research Article
Seismic Performance of Offshore Piers under Wave Impact and Chloride Ion Corrosion Environment
Table 5
Time-varying diameter and section loss rate of pier reinforcement in splash area under different service life.
| Service life (years) | 0 | 10 | 20 | 30 | 40 | 50 |
| Longitudinal bar | Diameter (mm) | 28 | 26.60 | 25.97 | 24.84 | 23.46 | 21.61 | Section loss rate (%) | 0 | 9.75 | 13.97 | 21.30 | 29.80 | 40.43 |