Experimental Study of Blast Resistance on BFRP Bar-Reinforced Cellular Concrete Slabs Fabricated with Millimeter-Sized Saturated SAP

Table 5

Crack width of slabs.

IDCrack width (mm)
Front surfaceBack surface

SP2-10.051.05
SP2-20.11.4
SP2-30.251.85
BS1-12.50.95
BS1-2
BS2-10.10.15
BS2-20.250.35
BS2-3
BS3-10.050.1
BS3-20.250.35
BS3-30.350.35