Research Article
High-Temperature Corrosion Behavior of Incoloy 800H Alloy in the Impure Helium Environment
Figure 1
(a) The schematic drawing of the system for high-temperature corrosion under impure helium and (b) the actual picture of the experimental facilities: (1) pure gas cylinder, (2) injection equipment for pure gas consisting of multiple mass flow controllers, (3) vacuum pump, (4) high-pressure gasholder, (5) mass flow controllers, (6) high-temperature furnace, (7) gas chromatography, and (8) water analyzer.
(a) |