Mix proportion of cement pastes.

SampleDosage of NC (%)Dosage of SAP (%)Influencing factor

0.30SJ0.3000
0.35SJ0.3500
0.40SJ0.4000

0.30SJ_NC0100.301.00NC content
0.30SJ_NC0150.301.50
0.30SJ_NC0200.302.00
0.30SJ_NC0300.303.00

0.30SJ_NC015S150.301.50.15SAP content
0.30SJ_NC015S300.301.50.30