Cooling data for the rhombohedral phase of PbNb2O6, from 700°C to 410°C: (a) temperature dependence of the real part of dielectric constant (), inset (b) temperature dependence of the imaginary part of dielectric constant (), and (c) temperature dependence of the dielectric loss (), at various frequencies (1 kHz to 5.5 MHz).