Research Article

Behavior of Yb3+ and Er3+ during Heat Treatment in Oxyfluoride Glass Ceramics

Figure 4

XRD patterns of (a) SA1.8EY and (b) SA2.18EY samples which were heat treated at 630, 660, 675, and 690°C for 48 hours.
171045.fig.004a
(a)
171045.fig.004b
(b)