Research Article
Metallurgical and Machinability Characteristics of Wrought and Selective Laser Melted Ti-6Al-4V
Figure 6
SEM image of cutting tool after machining (a) wrought and (b) SLM Ti-6Al-4V at = 180 m/min; = 0.1 mm/rev; and = 0.5 mm for 378 seconds.
(a) |
(b) |