Research Article
Conversion of Mill Scale Waste into Valuable Products via Carbothermic Reduction
Table 6
Mill scale experimental runs (reducing agent: graphite).
| Heat number | Stoichiometric carbon | Chemical composition of produced metal, wt% | C | Si | Mn | S | P |
| 9 | 0.7 | 0.014 | 0.0009 | 0.033 | 0.0835 | 0.0003 | 10 | 0.8 | 0.167 | 0.0009 | 0.048 | 0.0498 | 0.0103 | 11 | 0.9 | 2.33 | 0.0015 | 0.198 | 0.0322 | 0.0015 | 12 | 1.0 | 2.98 | 0.0454 | 0.353 | 0.0143 | 0.0169 | 13 | 1.1 | 3.36 | 0.0038 | 0.347 | 0.0100 | 0.0109 | 14 | 1.2 | 3.79 | 0.0294 | 0.283 | 0.0151 | 0.0109 | 15 | 1.3 | 3.80 | 0.1620 | 0.471 | 0.0104 | 0.0105 | 16 | 1.5 | 3.79 | 0.2450 | 0.464 | 0.0109 | 0.0117 |
|
|