Research Article

Aging Behaviour of Al-Mg-Si Alloys Subjected to Severe Plastic Deformation by ECAP and Cold Asymmetric Rolling

Figure 2

Representative TEM images and corresponding SAD patterns of the ultrafine structure achieved after (a) 6 ECAP passes and (b) asymmetric rolling reduction corresponding to 5,50 equivalent strain.
959643.fig.002a
(a)
959643.fig.002b
(b)