Research Article
Transition in Deformation Mechanism of AZ31 Magnesium Alloy during High-Temperature Tensile Deformation
Figure 3
Nominal-stress-nominal-strain curves for tensile deformation at 523 K (a), 573 K (b), and 623 K (c) at an initial strain rate of to 10−4 s−1.