Target density (kg/m3)Sand (kg/m3)Fly ash (kg/m3)Silica fume (kg/m3)AS/binderNaOH/Na2SiO3SP %wt of binderAl %wt of solidMolarity (M)

AGCF5505181841.8210.128
AGCFS55051892921.8210.128
AGCFP5505181841.82120.128