Growth of Zinc Oxide Nanorods with the Thickness of Less than or Equal to 1 μm through Zinc Acetate or Zinc Nitrate for Perovskite Solar Cell Applications

Table 3

FWHM analysis of the (002) XRD peak in ZnO NRs grown from the ZN source.

ParametersZN 0 minutesZN 15 minutesZN 60 minutesZN 90 minutesZN 120 minutes

Peak position (°)34.5134.4734.4834.5034.50
FWHM (°)0.370.390.380.370.36
Crystallite size (nm)20.3819.2919.8520.7920.94