FWHM analysis of the (002) XRD peak in ZnO NRs grown from the ZA source.

ParametersZA 0 minutesZA 15 minutesZA 60 minutesZA 90 minutesZA 120 minutes

Peak position (°)34.5134.5134.5034.5034.50
FWHM (°)0.710.370.360.360.35
Crystallite size (nm)10.7020.5721.0921.0621.62