Influence of Al2O3, CaO/SiO2, and B2O3 on Viscous Behavior of High Alumina and Medium Titania Blast Furnace Slag
Table 1
Chemical compositions of slag samples (wt.%).
| Number | CaO | SiO2 | MgO | Al2O3 | TiO2 | FeO | V2O5 | MnO | B2O3 | C/S |
| Basic slag | 28.33 | 24.85 | 8.64 | 14.24 | 19.48 | 1.11 | 0.20 | 0.65 | — | 1.14 | R1 | 29.76 | 24.04 | 9.27 | 13.77 | 18.84 | 1.07 | 0.19 | 0.63 | — | 1.24 | R2 | 31.46 | 23.45 | 9.06 | 13.44 | 18.38 | 1.05 | 0.19 | 0.62 | — | 1.34 | R3 | 33.02 | 22.91 | 8.87 | 13.13 | 17.95 | 1.02 | 0.18 | 0.60 | — | 1.44 | A1 | 27.45 | 24.08 | 9.28 | 15.98 | 18.87 | 1.08 | 0.19 | 0.63 | — | 1.14 | A2 | 27.12 | 23.79 | 9.18 | 17.00 | 18.64 | 1.06 | 0.19 | 0.63 | — | 1.14 | A3 | 26.78 | 23.50 | 9.08 | 18.01 | 18.41 | 1.05 | 0.19 | 0.62 | — | 1.14 | B1 | 27.12 | 23.79 | 9.18 | 16.00 | 18.64 | 1.06 | 0.19 | 0.63 | 1.00 | 1.14 | B2 | 26.45 | 23.20 | 8.98 | 17.02 | 18.18 | 1.04 | 0.19 | 0.61 | 2.00 | 1.14 | B3 | 25.80 | 22.64 | 8.78 | 17.97 | 17.74 | 1.01 | 0.18 | 0.60 | 3.00 | 1.14 | B4 | 25.13 | 22.05 | 8.58 | 19.00 | 17.28 | 0.98 | 0.18 | 0.58 | 4.00 | 1.14 |
|
|