Research Article
Using Externally Bonded CFRP to Repair a PCCP with Broken Wires under Combined Loads
Table 3
The five models.
| ||||||||||||||||||||||||||||||
1P is pipe, t is thickness, and the number indicates the number of layers of CFRP at 0.167 mm per layer. |
| ||||||||||||||||||||||||||||||
1P is pipe, t is thickness, and the number indicates the number of layers of CFRP at 0.167 mm per layer. |