Research Article
Monocrystalline Silicon PERC Solar Cell with Rear-Side AlOx Film Formed by Furnace Oxidation
Table 2
Electric parameters and conversion efficiencies measured for the Al-BSF cells (#1 to #3) and PERC (#A1 to #A3 and #B1 to #B3).
| | Jsc (mA/cm2) | Voc (mV) | FF (%) | (%) |
| Al-BSF #1 | 37.53 | 580.09 | 75.1 | 16.36 | Al-BSF #2 | 37.19 | 580.10 | 76.3 | 16.46 | Al-BSF #3 | 37.54 | 570.04 | 74.8 | 16.00 | PERC #A1 | 39.43 | 580.07 | 74.1 | 16.95 | PERC #A2 | 38.79 | 590.05 | 74.6 | 17.07 | PERC #A3 | 38.71 | 590.10 | 75.0 | 17.13 | PERC #B1 | 38.90 | 580.04 | 73.6 | 16.62 | PERC #B2 | 38.73 | 580.08 | 74.4 | 16.73 | PERC #B3 | 37.66 | 590.06 | 74.1 | 16.47 |
|
|