Research Article
Laminating Fabrication of Bifacial Organic-Inorganic Perovskite Solar Cells
Figure 3
Flow chart of bifacial PSCs: (a) deposition perovskite film on the SnO2 and NiO substrate, respectively; (b) lamination of the substrates together with pressure at 200°C for 15 min; (c) final device with perovskite films merging together; (d) photography of the devices.
(a) |
(b) |
(c) |
(d) |