Research Article

Growth of Hierarchically Structured High-Surface Area Alumina on FeCrAl Alloy Wires

Figure 4

Varied morphology when isothermally oxidized at 1000°C for 0.5 h–16 h.
251495.fig.004a
(a) 0.5 h
251495.fig.004b
(b) 1 h
251495.fig.004c
(c) 2 h
251495.fig.004d
(d) 4 h
251495.fig.004e
(e) 8 h
251495.fig.004f
(f) 16 h