Research Article

Corrosion Behavior of Candidate Structural Materials for Molten Salt Reactors in Flowing NaCl-MgCl2

Figure 6

The salt temperature during melting, stabilization, and normal operation of the natural convection loop. (a) The salt temperature up to first 20 h from the heater on. (b) An enlarged view between stabilization and normal operation. The experimental start time was defined as the moment when the temperature of T6 begins to rise from its lowest point.