Research Article

Titanium Oxide: A Bioactive Factor in Osteoblast Differentiation

Figure 3

SEM micrographs of hFOB 1.19 cells seeded on a glass coverslip (positive control), GTi and TiV (untreated alloys), TiV5 and GTi5 (500°C), TiV8 and GTi8 (800°C), MAOTiV (200 mA and 225 mA at 3 min and 4 min), and MAOGTi (200 mA and 225 mA at 3 min and 4 min) disks and incubated for 10 days (3 days at 33.5°C and subsequently 7 days at 39.5°C). Magnification 3500x.