Research Article

Deposition of Cerium-Based Conversion Coatings on Aluminum Alloy 380

Figure 5

Surface morphology of coatings deposited on panels rinsed at 25°C after immersion in the coating solution for (a) 2 min, (b) 5 min, and (c) 8 min.
760284.fig.005a
(a)
760284.fig.005b
(b)
760284.fig.005c
(c)