Research Article
Nanoclay Reinforced Ternary Blends Based on Biodegradable Polymers for Drug Delivery Application
Table 2
Erosion data for CS-PVA-PEG formulations.
| Formulation codes | Erosion (% ± SD) | pH 1.2 | pH 4.5 | pH 6.8 |
| MA7 | 71.57 ± 0.08 | 63.50 ± 0.10 | 61.77 ± 0.09 | MA8 | 72.25 ± 0.05 | 61.38 ± 0.10 | 59.16 ± 0.03 | MA9 | 75.94 ± 0.13 | 68.67 ± 0.08 | 66.60 ± 0.13 | MA10 | 74.51 ± 0.13 | 67.76 ± 0.08 | 66.50 ± 0.10 | MA11 | 73.07 ± 0.16 | 65.40 ± 0.26 | 63.88 ± 0.16 | MA12 | 73.82 ± 0.16 | 67.27 ± 0.13 | 65.52 ± 0.10 |
|
|