Research Article
Turning the Cocopith Waste into Myceliated Biocomposite to Make an Insulator
Table 5
Biocomposite press strength.
| No. | Specimens | Thickness (mm) | Width (mm) | Area (mm2) | Max load (N) | Maximum flexural stress (MPa) |
| 1 | Biocomposite 1 | 6.67 | 17.93 | 119.59 | 29.13 | 7.67 | 2 | Biocomposite 2 | 6.71 | 17.96 | 120.51 | 30.78 | 7.99 | 3 | Biocomposite 3 | 6.73 | 18.23 | 122.69 | 31.23 | 7.94 |
|
|