Selective Preconcentration of Gold from Ore Samples

Table 1

Effect of ligand concentration of retention of metal chelates.

Amount of DEBTAmount of Au3+ in sample solution (μg)% Sorption of gold chelates on resin

3mL of 2x10−3 mol L−115100 ± 2
3mL of 2x10−3 mol L−1100100 ± 2
3mL of 2x10−3 mol L−150094 ± 3

Amount of resin: 1.0 g, sample volume: 10 mL, and sample flow rate: 0.5 mL min−1.