Numerical Analysis on Flow Behavior of Molten Iron and Slag in Main Trough of Blast Furnace during Tapping Process

Figure 10

The molten iron lost in terms of the density phase at the slag port varying with the high difference of slag port to iron dam in the main trough of blast furnace: (a) 0.2 m; (b) 0.1 m; and (c) 0.05 m.