Research Article

Hot Deformation Behavior and Microstructural Evolution of Twin-Roll-Casting Mg Alloy during High-Temperature Compression

Table 2

True stress (MPa) of the TRC-AZ31 alloy during the stable stage at 500°C.

Strain (%)Sampling direction
10°

5292624
15252726
25282527
35272433