Polymer-Cement Mortar with Quarry Waste as Sand Replacement
Figure 12
Types of fractures in samples at 14 days. Mixtures (a) M1, (b) M3, (c) M7, (d) M8, and (e) M11 with higher performance, respectively, from the left side (own source).