Research Article
Study on the Effect of Different Fe2O3/ZrO2 Ratio on the Properties of Silicate Glass Fibers
Table 2
Mass and mass loss rate of samples before and after corrosion in NaOH solution.
| Sample | 1# | 2# | 3# | 4# | E-glass | AR-glass |
| /g | 10.5452 | 10.5235 | 10.5134 | 10.5012 | 10.5418 | 10.5057 | /g | 10.4693 | 10.4382 | 10.4083 | 10.3752 | 10.2761 | 10.4090 | Mass loss rate/% | 0.72 | 0.81 | 1.00 | 1.20 | 2.52 | 0.92 |
|
|