Research Article
Improvement of the Early-Age Compressive Strength, Water Permeability, and Sulfuric Acid Resistance of Scoria-Based Mortars/Concrete Using Limestone Filler
Figure 13
Water penetration depths measured in different concrete mixes cured for 2, 7, 28, and 90 days.