Research Article
Development and Characterization of Norite-Based Cementitious Binder from an Ilmenite Mine Waste Stream
Table 4
Compressive strength of the binders without any additives. The specimens were cured at 87°C and ambient pressure.
| Specimen 1 | Norite (g) | Alkali sol. | Wt. of alkali sol. (g) | L/S ratio | Curing time (days) | Estimated compressive strength (±2 MPa) |
| 300 | 8 M NaOH | 125 | 0.42 | 5 | 2.5 | 300 | 8 M NaOH | 125 | 0.42 | 7 | 3 | 300 | 8 M NaOH | 125 | 0.42 | 14 | 23 | 300 | 8 M NaOH | 125 | 0.42 | 28 | 24 |
|
|