Research Article

Chloride Diffusivity and Life Prediction of Cracked RC Beams Exposed to Different Wet-Dry Ratios and Exposure Duration

Table 8

and of different crack widths.

Crack width (10āˆ’12m2/s)

00 microns1.801.00
40 microns1.831.02
70 microns1.951.08
90 microns2.831.57
120 microns5.643.13