Names of RC beam specimens (Group A = 1 : 3, or B = 1 : 7, or D = 1 : 15).

Crack widthDuration
32 d48 d64 d96 d128 d144 d160 d

00 micronsA-00-32A-00-48A-00-64A-00-96A-00-128A-00-144A-00-160
40 micronsA-40-32A-40-48A-40-64A-40-96A-40-128A-40-144A-40-160
70 micronsA-70-32A-70-64A-70-96A-70-128A-70-160
90 micronsA-90-32A-90-64A-90-96A-90-128A-90-160
120 micronsA-120-32A-120-64A-120-96A-120-128A-120-160