Research Article
The Adhesion of CrN Thin Films Deposited on Modified 42CrMo4 Steel
Figure 17
Failure modes after Daimler–Benz test (left column) and 3D visualization of the selected indent morphology (right column) for CrN coatings deposited on (a) initial substrates, (b) shot-peened substrate (t = 600 s, p = 0.45 MPa), (c) nitrided substrate (tn = 3 h), and (d) shot-peened (t = 600 s, p = 0.45 MPa) and nitrided substrate (tn = 3 h).
(a) |
(b) |
(c) |
(d) |