Research Article
Experimental Study and Application of Inorganic Solidified Foam Filling Material for Coal Mines
Table 7
Experimental design of the sulphoaluminate cement content.
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Note. The gelling agent contained 0.1% water reducer; the water–cement ratio is the mass ratio of water to aggregate system; the gel-foam ratio is the ratio of the volume of the gel slurry to the volume of the foam. |