Effect of Filling Interval Time on Long-Term Mechanical Strength of Layered Cemented Tailing Backfill

Table 2

The uniaxial compressive strength of filling material for different layers (unit: MPa).

Specimen
number
Peak strength/MPaSpecimen
number
Peak strength/MPaSpecimen
number
Peak strength/MPaSpecimen
number
Peak strength/MPa

70-12-1/70-24-14.7370-36-13.8170-48-13.96
70-12-24.5170-24-23.2570-36-24.3470-48-22.5
70-12-34.3470-24-34.4270-36-33.9370-48-33.31
70-12-44.7170-24-44.1370-36-44.1770-48-43.82
70-12-53.5670-24-5/70-36-52.9670-48-53.82
70-12-6/70-24-63.2770-36-64.4170-48-6/
Average4.28Average3.95Average3.93Average3.48
72-12-14.2772-24-13.6372-36-14.1572-48-14.69
72-12-2/72-24-25.0272-36-23.5972-48-23.06
72-12-34.6172-24-3/72-36-33.7972-48-33.93
72-12-44.0672-24-44.5972-36-4/72-48-45.24
72-12-54.2372-24-5/72-36-54.5572-48-53.57
72-12-64.1172-24-63.6872-36-64.8472-48-63.82
Average4.26Average4.23Average4.18Average4.05
75-12-14.3975-24-15.8975-36-1/75-48-14.98
75-12-25.6975-24-23.8475-36-24.9675-48-25.49
75-12-35.6875-24-35.7375-36-35.3375-48-35.71
75-12-45.5475-24-45.4275-36-46.0175-48-45.17
75-12-56.2975-24-56.0775-36-5/75-48-55.25
75-12-65.8575-24-66.2575-36-65.5475-48-65.05
Average5.57Average5.53Average5.46Average5.28

Note: “/” is the largest value of the results and the average of strength value is calculated to promote a culling process.