Research Article
The Effect of Thermooxidative Aging on the Durability of Glass Fiber-Reinforced Epoxy
Figure 8
FTIR spectra of EHG250-68-37 composite sample in the hydroxyl and CH stretching regions (initially and after 800 h thermooxidative aging).