Research Article
Carbonation Coefficients from Concrete Made with High-Absorption Limestone Aggregate
Table 3
Concrete properties.
| w/c ratio | Designed strength MPa | Compressive strength MPa | Volumetric weight kg/m3 | Air % | Slump cm | Porosity % |
| 0.80 | 15 | 18.0 | 2,120 | 2.8 | 10 | 23.4 | 0.70 | 20 | 21.7 | 2,120 | 2.8 | 10 | 23.1 | 0.62 | 25 | 26.1 | 2,120 | 2.9 | 11 | 24.1 | 0.55 | 30 | 30.9 | 2,160 | 2.9 | 9 | 22.9 |
|
|