Research Article
High Field Linear Magnetoresistance Sensors with Perpendicular Anisotropy L10-FePt Reference Layer
Figure 4
The MR of the multilayer films measured at 300 K (a) and 10 K (b); (c) the linear magnetic field response of the multilayer films when the external field varies between +5 kOe and −5 kOe at 300 K. The insets in (c) show the three repeated measures of MR curve of the same sample.
(a) |
(b) |
(c) |