Phase Relations in (Ln = Nd & Sm) Electroceramics

Figure 1

SEM images of samples sintered at 1375°C for either 4 or 60 hours. Secondary electron images of (a) A0-4, (b) A0-60, (c) A6-4, and (d) A10-4 and matching backscattered electron images for (e) A10-4.
373079.fig.001a