Research Article
Mechanical Properties and Hardening Mechanism of Magnesium Ammonium Phosphate Cements Modified by Fly Ash
| Mixture ID | M + P (wt%) | Fly ash (wt%) | M/P | W/B | N/M (wt%) |
| FA0 | 100 | 0 | 3/1 | 0.20 | 12 | FA10 | 90 | 10 | 3/1 | 0.20 | 12 | FA20 | 80 | 20 | 3/1 | 0.20 | 12 | FA30 | 70 | 30 | 3/1 | 0.20 | 12 | FA40 | 60 | 40 | 3/1 | 0.20 | 12 | FA50 | 50 | 50 | 3/1 | 0.20 | 12 |
|
|