Research Article
Post-Fire Behavior of Modified SIFCON One-Way Plates with Waste Tire Rubber under Flexural Load: Experimental and Numerical Study
Table 7
Middle-third deflections of SIFCON specimens at service and ultimate load at 600°C.
| Specimen | The control specimen deflection at service load level (mm) | Percentage increase in deflection at service load (control specimen) | Deflection at ultimate load (mm) | Percentage increase in deflection at ultimate load (control specimen) |
| M1-F4 | 5.8 | — | 11.15 | — | M2-F4-P5 | — | — | 9.69 | 13.1 | M3-F4-P10 | — | — | 10.27 | 7.9 | M4-F4-P15 | — | — | 10.82 | 2.9 |
|
|