Post-Fire Behavior of Modified SIFCON One-Way Plates with Waste Tire Rubber under Flexural Load: Experimental and Numerical Study
Table 5
Ultimate load, deflection, and flexural strength of all SIFCON plates.
| Specimen | At 25°C | At 600°C | First crack load (Pcr) (kN) | Ultimate load (Pu) (kN) | Pcr/Pu (%) | First crack load (Pcr) (kN) | Ultimate load (Pu) (kN) | Pcr/Pu (%) |
| M1-F4 | 15.2 | 25.3 | 60.5 | 14 | 21.1 | 66 | M2-F4-P5 | 10.9 | 22.1 | 49.3 | 8.6 | 13.5 | 63.7 | M3-F4-P10 | 10.5 | 21.3 | 49.2 | 8.2 | 13 | 63 | M4-F4-P15 | 9.1 | 18.9 | 48.5 | 6.4 | 11.1 | 57.6 |
|
|