Research Article

Large Ring Test for Evaluation of Restrained Shrinkage Cracking: Calibration and Experimental Trial

Figure 8

Scatter plot showing corrected circumferential strain on the inner surface of Ring A’s steel ring within the first 2 days (12 measurements per minute), along with the temperature of the steel ring measured using a thermocouple.